1=Excellent, 3=Very Good, 6=Average, 10=Poor
Guidelines
Coating SelectionCHART
PROPERTY | EPOXY | EPOXY-POLYESTER (HYBRID) 50/50 | EPOXY-POLYESTER (HYBRID) 60/40 | EPOXY-POLYESTER (HYBRID) 70/30 | POLYESTER TGIC | POLYESTER TGIC FREE | SUPER DURABLE | PU |
---|---|---|---|---|---|---|---|---|
Adhesion | 2 | 3 | 3 | 3 | 3 | 3 | 3 | 3 |
Appearance | 4 | 5 | 4 | 3 | 4 | 4 | 3 | 2 |
Aliphatic Hydrocarbon | 2 | 3 | 3 | 3 | 4 | 4 | 4 | 2 |
Boiling Resistance | 3 | 3 | 4 | 5 | 3 | 4 | 4 | 4 |
Detergent Resistance | 1 | 3 | 4 | 5 | 5 | 7 | 6 | 5 |
Flexibility | 3 | 5 | 4 | 3 | 3 | 2 | 5 | 3 |
Heat Resistance | 5 | 4 | 4 | 4 | 2 | 2 | 2 | 1 |
Humidity Resistance | 2 | 3 | 4 | 5 | 6 | 5 | 5 | 5 |
Impact Resistance | 3 | 4 | 4 | 3 | 3 | 2 | 8 | 3 |
Pencil Hardness | 2 | 2 | 3 | 4 | 5 | 5 | 5 | 5 |
Salt Spray | 1 | 3 | 4 | 5 | 5 | 5 | 4 | 5 |
Stain Resistance | 3 | 3 | 4 | 4 | 5 | 5 | 6 | 5 |
UV Colour Change | 8 | 8 | 7 | 7 | 3 | 3 | 2 | 3 |
10% Sodium Hydroxide | 3 | 3 | 4 | 5 | 5 | 7 | 7 | 4 |
10% Hydroelectric Acid | 4 | 4 | 5 | 5 | 4 | 5 | 5 | 5 |
Coverage : (1) 10-12 Square meters per kg at 50-60 microns dry film thickness.
(98%, Utilisation) (2) 6-8 Square meters per kg for Structures, Textures, Hammertone and Antiques.
Packing : 10 & 20 kgs in corrugated box
Storage : PURECOAT powders should be stored in a cool and dry place. The shelf life of the powder is minimum 6 months when stored at 30 deg.°c and approx.
60 % RH.in closed carton powder shelf life is reduced at high temperature.
Application : Electrostatic (Corona) spray gun(50-90KV gun voltage for non – metallic and 20-50 KV for all metallic powders), Tribo gun Fluidized bed and Chamber coating.
Baking Schedule : Normally 200 deg.°c /10-12 Minutes for PP and 180 deg.°c / 10-12 Minutes for Epoxy and Hybrid.
(EMT) For exact baking, please read sticker on each box.